Meaning
Mechanical characterization of a material’s resistance to localized plastic deformation is conducted by applying a low force to a diamond indenter of specific geometry. The resulting microindentation hardness value is calculated from the ratio of the applied load to the surface area of the permanent impression.
Measurement Method
Testing protocols typically employ loads ranging from one to one thousand grams-force to produce small, localized impressions. Determining the microindentation hardness involves measuring the diagonals of the indent using optical microscopy or a high-resolution imaging system. The Vickers or Knoop scale is then used to quantify the hardness value based on the measured dimensions.
Accuracy in these measurements is highly dependent on sample preparation and optical resolution.
Deformation Mode
Elastic recovery occurs when the indenter is unloaded, which can alter the final dimensions of the impression. In brittle materials, microindentation hardness testing can initiate microcracking at the corners of the indent. This cracking behavior provides data that enables estimation of the fracture toughness of the specimen.
Careful analysis of this response prevents misinterpretation of the hardness values obtained from brittle ceramics.
Surface Sensitivity
Surface preparation holds paramount importance in low-load testing because the depth of the indent is often under a few micrometers. Polishing the specimen to a mirror-like finish is necessary to eliminate work-hardened surface layers that would skew the microindentation hardness results toward artificially high values. Inhomogeneous regions or thin coatings can also be resolved using these shallow indents.
Accurate surface control ensures the reproducibility of the hardness profiles across the material cross-section.