Meaning
Polymer degradation during processing involves the breaking of long-chain molecules into shorter fragments due to excessive heat or shear. This phenomenon, referred to as molecular weight loss, reduces the mechanical strength and impact resistance of the molded part. It is often caused by high melt temperatures or long residence times in the barrel.
When the resin is exposed to these harsh environments, the thermal energy overcomes the carbon-carbon bonds, leading to chain scission and a shift in the material properties.
Processing Variable
High shear rates in narrow gates generate intense localized heat. Under these conditions, molecular weight loss accelerates and weakens the material. Moisture in the resin also triggers hydrolytic degradation.
Proper drying before processing prevents this reaction from occurring.
Mechanical Consequence
Parts molded from degraded resin suffer from brittleness and reduced wear resistance. When molecular weight loss is high, the material fails to meet the specified impact performance. This change in physical properties causes premature failures in the field.
Testing for this degradation is completed using melt flow index measurements.
Quality Audit
Verifying that the molding process has not degraded the material involves comparing the viscosity of the raw resin with that of the molded part. A significant increase in the melt flow rate indicates that polymer chain scission has occurred. This assessment is necessary when using recycled regrind.